HOT-COLD
IMPREGNATION
OF METAL POROSITY
|
|
Check
out our products selector guide
With
full technical details
COLD IMPREGNATION
METAL POROSITY IMPREGNATION RESISN
|
70-11
|
ROOM
TEMPERATURE CURING IMPREGNATION RESIN
|
|
STEP 1
|
VACUUM
|
|
STEP 2
|
IMPREGNATION BY IMMERSION
|
|
STEP 3
|
CENTRIFUGAL WASH
|
|
STEP 4
|
DRYING
|
|
STEP 5
|
POLYMERIZATION AT AMBIENT CONDITIONS
|
HOT
IMPREGNATION METAL POROSITY IMPREGNATION RESISN
|
70-90
|
HOT WATER 90 °C CURING IMPREGNATION RESIN
|
|
STEP 1
|
VACUUM
|
|
STEP 2
|
IMPREGNATION BY IMMERSION
|
|
STEP 3
|
CENTRIFUGAL WASH
|
|
STEP 4
|
POLYMERIZATION IN HOT WATER
|
|
STEP 5
|
DRYING
|
HOT IMPREGNATION
METAL POROSITY IMPREGNATION RESISN
|
70-91
|
RECYCLABLE HOT CURING IMPREGNATION RESIN, DESIGNED
TO BE RECOVERED FROM WASHING WATER
|
|
STEP 1
|
VACUUM
|
|
STEP 2
|
IMPREGNATION BY IMMERSION
|
|
STEP 3
|
CENTRIFUGAL WASH
|
|
STEP 4
|
POLYMERIZATION IN HOT WATER
|
|
STEP 5
|
DRYING
|